Nickel-plated aluminium sample plate with a uniform satin surface

Finishing guide

Electroless vs electroplated nickel: which to specify

"Nickel plating" refers to two distinct processes: electroless and electroplated. They behave differently, and the right choice depends on your part's geometry and how uniform the coating must be.

Side by side

Typical behaviour. We confirm it against your spec at quoting.
 Electroless nickel (ENP)Electroplated nickel
How it's depositedChemical (autocatalytic) bathElectric current
Thickness uniformityEven everywhere — bores, threads, recessesHeavy on edges, thin in recesses/bores
Typical thickness8–25 µm~5–40 µm (uneven)
HardnessHigh (higher after a high-temp bake)Moderate
CorrosionHighModerate–high
LookUniform satinBright, cosmetic
Cost$$$$$
Best forComplex parts, deep features, hardness, all-over thicknessSimple shapes, bright look, lower cost

Electroless (ENP)

Because the metal is deposited by a chemical reaction rather than by electric current, it builds the same thickness on every surface — the inside of a deep bore is coated as evenly as an outside edge. The deposit is a hard, wear-resistant nickel-phosphorus alloy, and a high-temperature bake (~340–400 °C) hardens it further still — though on age-hardened aluminium like 6061/7075 the bake is kept low to protect the temper, so there it mainly improves adhesion and relieves stress. That makes electroless the right choice for complex geometry and for any part where the plated thickness has to stay in tolerance everywhere.

Electroplated

Electroplating is faster, lower in cost, and produces a bright, cosmetic finish. The limitation is inherent to the process: the electric current concentrates on edges and corners, so the coating builds up thick there and remains thin inside bores and recesses. It suits simple shapes where appearance or cost is the priority.

Plating aluminium

Aluminium grades like 6061 and 7075 won't accept nickel directly — they need a pre-treatment called a zincate step that prepares the surface for either process. We confirm the exact spec at quoting.

Coatings mirror the surface: plating reproduces the texture beneath it. A part finished at Ra 1.6 remains Ra 1.6 after nickel — tool marks included. For a smoother result, we polish or brush the part before plating rather than after.
A practical point from our shop floor: when a part has deep bores or threads that must hold tolerance after plating, electroless is the better choice — there is no edge build-up to mask off or grind back.

Three quick mistakes

  • Expecting plating to smooth a rough surface — it mirrors what's underneath, so finish the part first.
  • Not stating a thickness or a spec — for electroless nickel, call out ASTM B733.
  • Forgetting that the coating adds thickness — it eats into tight bores and close fits.

Quick rule

Complex geometry, uniform coverage, or hardness → electroless. Simple shape, a bright look, or lower cost → electroplated.

Send your part — we'll recommend the right plating See the Finish Library
Nickel-plated CNC parts in protective foam packaging

Pick the right nickel

We'll recommend the plating at quoting.

Send your part and target spec, we'll recommend electroless or electroplated nickel and quote in 48 hours.